물성표
Durability at pressing, kg/㎠ | Coefficients | |||||||
---|---|---|---|---|---|---|---|---|
Average density kg/m |
Porosity, % |
Water sorption, % |
In dry state | In waterlogged state | After 25 cycles | Softening | Frost resistance | |
ARMENIAN GOLD | 1867 | 23.8 | 10.67 | 409 | 319 | 259* | 0.78 | 0.8 |
ARMENIAN GOLD | ||
---|---|---|
Average density kg/m |
1867 | |
Porosity, % |
23.8 | |
Water sorption, % |
10.67 | |
Durability at pressing, kg/㎠ | In dry state | 409 |
In waterlogged state | 319 | |
After 25 cycles | 259* | |
Coefficients | Softening | 0.78 |
Frost resistance | 0.8 |
시공사례